Refractories for Iron Making
Refractories for Steel Making
| Item | RL-65 | RL-55 | RL-48 | |
| Al2O3 (%) | ≥65 | ≥55 | ≥48 | |
| Refractoriness (℃) | ≥1790 | ≥1770 | ≥1750 | |
| 0.2Mpa Refractoriness Under Load (℃) | ≥1500 | ≥1470 | ≥1420 | |
| Linear Change on Reheating (%) | 1500℃*2h | +0.1 | -0.4 | -- |
| 1450℃*2h | -- | +0.1 | -0.4 | |
| Apparent Porosity (%) | ≤24 | |||
| Cold Crushing Strength (MPa) | 49.0 | 44.1 | 39.2 | |