Refractories for Iron Making
Refractories for Steel Making
Item | Fireclay Insulation Brick | ||||
NG-0.5 | NG-0.6 | NG-0.8 | NG-1.0 | NG-1.2 | |
Al2O3(%) ≥ | 35 | 40 | 42 | 42 | 42 |
Fe2O3(%) ≤ | 2.5 | 2.5 | 2.0 | 2.0 | 2.0 |
Bulk Density (g/cm3) ≤ | 0.5 | 0.6 | 0.8 | 1.0 | 1.2 |
Cold Crushing Strength(MPa) ≥ | 1.0 | 1.5 | 2.0 | 2.5 | 3.0 |
Linear Change On Reheating 2% (℃*h) ≤ |
1000℃*12h | 1100℃*12h | 1150℃*12h | 1200℃*12h | 1200℃*12h |
Thermal Conductivity (w/m.k,{350±25℃})≤ |
0.18 | 0.25 | 0.35 | 0.50 | 0.52 |
Maximum Use Temperature (℃) ≥ | 1000 | 1100 | 1150 | 1200 | 1200 |